Do you mean when making the mould? Not normally. You mould on a fabricated flange for part one, demould the flange when ready to make part 2, release coat your mould flange then part 2 gets laid up directly onto the flange of part one. That way the parts are perfectly fitting and because youve release coated the flange on part one, the 2 mould halves will separate easily.