Group: Forum Members
Posts: 1,
Visits: 20
|
Hi guys I am new here and I am hoping I can get some good insight from people with more knowledge and experiences than myself. I have a part that I am trying to cover one side of with an image. The American flag and I want the back to retain it carbon fiber look on the other side and of course the strengths and light weight aspects. I tried using a shirt that had a flag on it and adding it as the first layer in the hand layup process and it turned the white to a grey. The other colors retained there apperance. I would be adding many different images to many parts and I need a good soild solution would also love to incorporate my logo as well. Will be using resin infusion over hand layup here soon if that makes a difference. Thanks in advance!
|