There can be several reasons for the cured resin sweating. Slight inaccuracy of either part A or part B when measured can lead the excess component being sweated out. Improper remixing of the settled sediment can cause it too. Other issues can be the resin isn't quite fully cured which is usually a temperature issue so a quick post cure will solve that.