MEKP Ratio


Author
Message
aliwes
a
Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)Supreme Being (201 reputation)
Group: Forum Members
Posts: 7, Visits: 17
Hello all,

Today I started to make some small car part moulds - headlight bowl and indicator pod. Anyway, I quickly realised that the digital scales that I bought from EC are not sensitive enough to do a mix of 50-100g of Coupling coat.

Is there any info on the number of ml per gram? I have a syringe which will make the job much more accurate. I know 1 gram go water is 1ml so shall I assume the same for the MEKP?

Cheers

Al