What type of adhesive should I use to bond a glassfibre / Polyester component to a wooden structure?
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
An epoxy adhesive would be my choice, though polyurethane would bond well too. Both are quite easy to bond to, just prep the surfaces well.