Ideal vacuum level for cosmetic parts


Author
Message
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Dezer - 2/16/2018 2:59:09 AM
hello friends, I already tried to process the vacuum bag, but it was disastrous because it removed more resin than it should have. What is the correct vacuum for hand layup + vacuum bag?

I do not have vacuum pump pressure regulator, any suggestions of what I can do?

You can add a new ball valve or similar your pump line and adjust it so that it leaks to any level you want. Still no regulator but it is an adjustable set up.
Wet layups need far less pressure than infusion or pre pregs. 10"hg





Edited 8 Years Ago by Fasta
Dezer
Dezer
Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
hello friends, I already tried to process the vacuum bag, but it was disastrous because it removed more resin than it should have. What is the correct vacuum for hand layup + vacuum bag?

I do not have vacuum pump pressure regulator, any suggestions of what I can do?