Good evening

I was wondering if it is possible to make a part that needs a split mould without the use of a curing oven. The latter is pretty much keeping me from trying prepregs as I can't use my domestic oven because I can't get a vacuum line in there and buying one isn't in the budget. Getting an old domestic oven just for this purpose where I can make a hole would be possible but I also don't really have the space for setting up a second oven...

My idea was to use a very slow curing hardener, i.e 210 or 300 minutes, and then hand lay up the carbon and epoxy inside the two parts before closing them and then add the vacuum bag and just wait until it's cured. I think the curing time would be plenty long enough but the big question is will the hand layup stick well enough to the mould so that it doesn't come loose in the process or how can it be made to stick well enough? Has anyone done this and can share some experiences?

Kind regards
Martin

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
atlantis - 8 Years Ago
MarkMK - 8 Years Ago
atlantis - 8 Years Ago
Weaponofchoice - 8 Years Ago
oekmont - 8 Years Ago
atlantis - 8 Years Ago
oekmont - 8 Years Ago
atlantis - 8 Years Ago
oekmont - 8 Years Ago
MarkMK - 8 Years Ago
oekmont - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search