Group: Forum Members
Posts: 4,
Visits: 13
|
Hello, I'm currently making brackets for kart parts by the means of resin infusion. I have successfully created a 3mm thick metre square piece with perfect finish etc. I have purchased a line bender for plexiglass etc for simple bracket mould making. I am using 4mm clear low impact polystyrene as my mould. The bend works perfect, however when I apply easylease chemical release agent it appears to shock the bend and hundreds of small cracks appear across the bend only. The rest of the sheet work fine. The release agent and sheet are the same temperature (20). Could this be an incompatible release agent for clear polystyrene? Should I use a higher grade of thermo plastic sheet and a wax release agent instead? Please help!
|