OV301 Precision Composites Curing Oven - [SOLVED]


Author
Message
Lode D
Lode D
Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)
Group: Forum Members
Posts: 5, Visits: 21
We recently bought the OV301 curing oven for use in our lab as an infusion oven.
Trying to install today, but we have encountered several problems. First of all, the accompanying manual is very unclear. Basically, we are not able to set the oven to a fixed temperature, no matter what we try. Following the instructions in the manual results in different outcomes than described in the manual itself.... Furthermore, the oven displays all kinds of messages (abbreviations since there are only a few digits) when pressing buttons, but nowhere there is an overview of what each message/abbreviation actually means. It even seems that some messages are not even how they should be, e.g. our oven displays "CnPt" instead of "InPt" (input).

Could you provide a schematic overview of the oven controls?
At least, we would be able to see then "where" we are in the menu. This would make it a lot easier to navigate the controls on the oven.
Hopefully, we'll be able to set the oven then to the single temperature mode (which currently does not work).

I can also not find a digital copy of the manual on your site, maybe this can be a good addition so that people are not dependent on one hardcopy which will eventually be outdated.

Our alarm light also seems to be on all the time. Sometimes there is a very annoying and loud sound (the oven itself is not warming up, still at ambient temperature, so the alarm is not related to any temperature overshoot). Nowhere in the manual can I find how to turn off the alarm (or at least the sound).


Edited 8 Years Ago by Lode D
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lode D - 8 Years Ago
Stacy (Staff) - 8 Years Ago
Lode D - 8 Years Ago
Stacy (Staff) - 8 Years Ago
Lode D - 8 Years Ago
Stacy (Staff) - 8 Years Ago
Lode D - 8 Years Ago
Lode D - 8 Years Ago