If I was making a cover for something (using resin infusion) where there was no strength needed and wanted to keep it as thin as possible, would it acceptable to just use single ply carbon fibre? Or would the minimum be 2 ply?

Cheers Tony
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can infuse a single layer of fabric. However you will need to be careful removing the peel ply and infusion stack to avoid damaging the fabric.  It can help to use a perforated release film between the peel ply and mesh to aid removal.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TonyW
T
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 12, Visits: 34
Warren (Staff) - 1/30/2018 11:05:14 AM
You can infuse a single layer of fabric. However you will need to be careful removing the peel ply and infusion stack to avoid damaging the fabric.  It can help to use a perforated release film between the peel ply and mesh to aid removal.

Cheers. Think I'll just  play it safe and go 2 ply. 