DIY Curing Oven help


Author
Message
KOSTAS
KOSTAS
Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)Supreme Being (493 reputation)
Group: Forum Members
Posts: 30, Visits: 244
Steve Broad - 3/27/2018 5:09:08 PM
janardian - 2/27/2018 7:25:19 PM
Michael Guilford - 2/27/2018 4:23:49 PM
bit of a late reply.
But  my curing oven is made from  100mm  foil backed insulation board. with a piece of tilebacker on the base for durability and heat distribution

I  have wired two 2000w heating elements in series to bring power down to 500w and use a thermostat to regulate temperature. You could also use a PWM controller to regulate power.

The fan motor is on the outside (would overheat inside). I use a tiny 12v van with a RC plane prop as a fan, connected through the walls.



Thank you for your answer! every bit helps!

Mine is made from ply sheet and 50mm insulation and silver foil. Heat is supplied by 4 separate circuits powering 150w bulbs. one of these circuits is connected to an adjustable thermostat, allowing me to control oven temps. Used an old metal desk fan with the motor in the wall :-)


 




Old microwave glass for viewing progress. Controls and wiring is a little bit Heath Robinson, but it works and I might tidy it up some day (probably not :-) ) If you look between the rows of switches you can see some of the remote temp sensors that allow me to check that I am getting an even cook.


Oven built to take front clip of my car. It fits, just . Photo has loaded sideways for some reason :-(





how it is called the internal silver lining and where should i look to find it ? thank you

Barnsley-Bill
B
Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)Supreme Being (310 reputation)
Group: Forum Members
Posts: 25, Visits: 489
Hi I've just received my CN7800 pid controller and there is a small jumper in the box and download software ' how dose the pid controller receive data from the software and what is the jumper for as I can't see anywhere were it goes 
Thanks  
Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
janardian - 4/11/2018 3:25:02 AM
Steve Broad - 4/8/2018 9:46:45 PM
janardian - 4/8/2018 9:33:38 PM
Steve Broad - 4/8/2018 7:27:12 PM
Are you still thinking of building an autoclave? If so, I strongly suggest that you don't!  For example, a 1m x 1m x 1m oven would experience, at only 1 atmosphere of pressure (around 14 .7psi and what can be achieved using a vacuum bag), 134,000lb of force! Basically a home made bomb !!!

No just an oven! I messed up in some of the wording - and yeah I agree that would be very dangerous to DIY with no experience!
We use vacuum bags and the oven for curing. Since we're a student club with very little resources, the prepreg we get is usually donated by a company and that dictates the cure cycle and temperature; autoclave would be ideal but yeah impractical, so we are currently using a makeshift oven. We're trying to find benefactors who might donate out of autoclave prepreg instead, since that seems a lot more reasonable!


Phew! :-)

You are using autoclave prepreg in an oven? What are the results like? Any photos? Where are you?

We're from UCLA and we're competing this year at the SAMPE student bridge contest! Although this is our third year participating, this is the first time we are trying to be fully self-sufficient! I will post pictures and updates soon!

OK, look forward to seeing them.

With regard to cheap prepreg - I have just received 11m2 of 270gsm prepreg for the cost of shipping only! The company had some out of date material that they couldn't sell. However, the storage life is similar to food storage Best Before times. The stuff remains usable for a lot longer than the 12 months stated. Maybe worth contacting local suppliers to see if they have any out of date OOA material they would be prepared to donate.

janardian
j
Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)
Group: Forum Members
Posts: 15, Visits: 105
Steve Broad - 4/8/2018 9:46:45 PM
janardian - 4/8/2018 9:33:38 PM
Steve Broad - 4/8/2018 7:27:12 PM
Are you still thinking of building an autoclave? If so, I strongly suggest that you don't!  For example, a 1m x 1m x 1m oven would experience, at only 1 atmosphere of pressure (around 14 .7psi and what can be achieved using a vacuum bag), 134,000lb of force! Basically a home made bomb !!!

No just an oven! I messed up in some of the wording - and yeah I agree that would be very dangerous to DIY with no experience!
We use vacuum bags and the oven for curing. Since we're a student club with very little resources, the prepreg we get is usually donated by a company and that dictates the cure cycle and temperature; autoclave would be ideal but yeah impractical, so we are currently using a makeshift oven. We're trying to find benefactors who might donate out of autoclave prepreg instead, since that seems a lot more reasonable!


Phew! :-)

You are using autoclave prepreg in an oven? What are the results like? Any photos? Where are you?

We're from UCLA and we're competing this year at the SAMPE student bridge contest! Although this is our third year participating, this is the first time we are trying to be fully self-sufficient! I will post pictures and updates soon!

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
janardian - 4/8/2018 9:33:38 PM
Steve Broad - 4/8/2018 7:27:12 PM
Are you still thinking of building an autoclave? If so, I strongly suggest that you don't!  For example, a 1m x 1m x 1m oven would experience, at only 1 atmosphere of pressure (around 14 .7psi and what can be achieved using a vacuum bag), 134,000lb of force! Basically a home made bomb !!!

No just an oven! I messed up in some of the wording - and yeah I agree that would be very dangerous to DIY with no experience!
We use vacuum bags and the oven for curing. Since we're a student club with very little resources, the prepreg we get is usually donated by a company and that dictates the cure cycle and temperature; autoclave would be ideal but yeah impractical, so we are currently using a makeshift oven. We're trying to find benefactors who might donate out of autoclave prepreg instead, since that seems a lot more reasonable!


Phew! :-)

You are using autoclave prepreg in an oven? What are the results like? Any photos? Where are you?
janardian
j
Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)
Group: Forum Members
Posts: 15, Visits: 105
Steve Broad - 4/8/2018 7:27:12 PM
Are you still thinking of building an autoclave? If so, I strongly suggest that you don't!  For example, a 1m x 1m x 1m oven would experience, at only 1 atmosphere of pressure (around 14 .7psi and what can be achieved using a vacuum bag), 134,000lb of force! Basically a home made bomb !!!

No just an oven! I messed up in some of the wording - and yeah I agree that would be very dangerous to DIY with no experience!
We use vacuum bags and the oven for curing. Since we're a student club with very little resources, the prepreg we get is usually donated by a company and that dictates the cure cycle and temperature; autoclave would be ideal but yeah impractical, so we are currently using a makeshift oven. We're trying to find benefactors who might donate out of autoclave prepreg instead, since that seems a lot more reasonable!

Steve Broad
Steve Broad
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Are you still thinking of building an autoclave? If so, I strongly suggest that you don't!  For example, a 1m x 1m x 1m oven would experience, at only 1 atmosphere of pressure (around 14 .7psi and what can be achieved using a vacuum bag), 134,000lb of force! Basically a home made bomb !!!
janardian
j
Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)
Group: Forum Members
Posts: 15, Visits: 105
Hanaldo - 4/8/2018 6:58:00 AM
Just look at any replacement fan and motor unit for any model oven and adapt it to fit your oven. The thing you need is a fan mounted on an extended shaft so that you can have the motor mounted externally to the oven. 

I see, thanks!!

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Just look at any replacement fan and motor unit for any model oven and adapt it to fit your oven. The thing you need is a fan mounted on an extended shaft so that you can have the motor mounted externally to the oven. 
janardian
j
Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)Supreme Being (485 reputation)
Group: Forum Members
Posts: 15, Visits: 105
Steve Broad - 3/27/2018 5:09:08 PM
janardian - 2/27/2018 7:25:19 PM
Michael Guilford - 2/27/2018 4:23:49 PM
bit of a late reply.
But  my curing oven is made from  100mm  foil backed insulation board. with a piece of tilebacker on the base for durability and heat distribution

I  have wired two 2000w heating elements in series to bring power down to 500w and use a thermostat to regulate temperature. You could also use a PWM controller to regulate power.

The fan motor is on the outside (would overheat inside). I use a tiny 12v van with a RC plane prop as a fan, connected through the walls.



Thank you for your answer! every bit helps!

Mine is made from ply sheet and 50mm insulation and silver foil. Heat is supplied by 4 separate circuits powering 150w bulbs. one of these circuits is connected to an adjustable thermostat, allowing me to control oven temps. Used an old metal desk fan with the motor in the wall :-)


 




Old microwave glass for viewing progress. Controls and wiring is a little bit Heath Robinson, but it works and I might tidy it up some day (probably not :-) ) If you look between the rows of switches you can see some of the remote temp sensors that allow me to check that I am getting an even cook.


Oven built to take front clip of my car. It fits, just . Photo has loaded sideways for some reason :-(




That is a really cool and interesting way to do it!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search