Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Welcome to the forum. Infusion is all about following the process to the letter and not moving on to the next stage until you are ready. The biggest difficulty is making sure your fabric is properly in the mould to avoid bridging and making sure you have a leak free bag. If you can get those two right then chances are the parts will come out very good.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|