Hi all


Author
Message
TonyW
T
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 12, Visits: 34
Warren (Staff) - 1/19/2018 5:08:32 PM
You can do it that way or do it corner to corner to make the resin flow a bit more practical. Sometimes the resin doesn't flow in a straight line.

Think I'll try corner to corner then. Want to make sure the part comes out right the first time. Cheers will let you know how it turns out. 

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can do it that way or do it corner to corner to make the resin flow a bit more practical. Sometimes the resin doesn't flow in a straight line.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TonyW
T
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 12, Visits: 34
Warren (Staff) - 1/19/2018 9:11:39 AM
Welcome to the forum.  Infusion is all about following the process to the letter and not moving on to the next stage until you are ready.  The biggest difficulty is making sure your fabric is properly in the mould to avoid bridging and making sure you have a leak free bag.  If you can get those two right then chances are the parts will come out very good.

Nothing worse than a leaky bag lol. The first part I'm looking to make is only about 2" wide but the full width of the car. I believe the resin has to travel the shortest distance so I would need to lay the feed tube the full length of the part. Firstly would this be correct and secondly should I bring the tube down either side too ensure it gets in to all the corners?

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Welcome to the forum.  Infusion is all about following the process to the letter and not moving on to the next stage until you are ready.  The biggest difficulty is making sure your fabric is properly in the mould to avoid bridging and making sure you have a leak free bag.  If you can get those two right then chances are the parts will come out very good.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TonyW
T
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 12, Visits: 34
Hi, although I've been messing around with fibre glass for years (mainly big bodykit back in the 90s) I've never actuly applied any specific measures or consistency to my resin mix. I' looking to make a few carbon fibre interior parts for my car. This will involve making moulds and eventually infusing the new parts. If I can achieve a finish even half as good as your you tube video on the bonnet I'll be happy with that. I just hope it' as easy as you guys make it look lol. 