continous duty vaccum pump


Author
Message
Andrey Revyakin
Andrey Revyakin
Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)Forum Member (32 reputation)
Group: Forum Members
Posts: 3, Visits: 5
Can you comment on which of your pumps would support continous-on operation overnight without overheating?

When I do vaccum bagging, I frequently get pinhole leaks from connectors etc which are difficult to debug. My parts are mostly long tubes of special shapes. All reagents come from you, except that, as a bag,  I use thick long polypropylene sleeves which I connect with your red standard disk-connector, and seal both ends with a hot wire. The leaks appear to be around the connector, and are hard to debug. So  I just set my oil-free pump on continous pumping. It has a feedback, so it switches on/off every 3 seconds to retain the vacuum, which causes overheating, and requires me to set-up a separate cooling fan. I am now considering to get a separate pump, and I am wondering how it would behave if left on cotinously for 12-16 hrs at a time.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Andrey Revyakin - 8 Years Ago
oekmont - 8 Years Ago
Warren (Staff) - 8 Years Ago
Andrey Revyakin - 8 Years Ago
oekmont - 8 Years Ago
Andrey Revyakin - 8 Years Ago
cumberdale - 8 Years Ago
Hanaldo - 8 Years Ago
cumberdale - 8 Years Ago
cumberdale - 8 Years Ago