I'm working on some CNC cut foam patterns, and after some advise on which products/methods to use to get a suitably surfaced pattern for taking the mould...

The surface isn't perfectly smooth, with many small pockets from the machining process - see attached image (slightly worse in places)

My original plan - (and have ordered these bits) was to use your epoxy coating resin with glass bead & silica and then brush/spray onto the surface - do you think that will be sandable to a suitable surface finish? should I be looking at adding some 163g woven glass over the part? These are largish parts for car bodywork...

Many Thanks,
James
Attachments
20120608_120833.jpg (814 views, 248.00 KB)
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
By hand would be the way to go when skinning a pattern like this. You actually want it to be resin rich so that you've got some resin to sand into so hand laminating is the right choice.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago
jamesw - 14 Years Ago
jamesw - 14 Years Ago
Matt (Staff) - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search