In an ideal world, you can degas the silicone in a degassing chamber but for simple casting it is not essential. Just "stretch pour" instead to remove the big bubbles. Stretch pouring is pouring from a height as a thin trickle of silicone to help remove the bubbles. If there is fine detail, you can also brush the silicone into the detail ensuring no air is trapped, then pour the main silicone pour. That way there is no air on the mould surface where it matters, but the rest might have bubbles.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|