Hi,
I'm trying to select a material to use with dry flowers, we have left over flowers from our wedding and we thought it would be nice to make them into a tabletop feature.
We are looking at table with raised sides as shown below:

Obviously we'll have to blank off the carry handles to avoid a great mess!
The main concerns are which material wont either ruin the paint on the table,or destroy the dry flowers, or have the flowers effect the clarity of the material.
I've looked at the Glass Cast Epoxy and the Water Clear Polyester Casting Resin but can't decide between the two, there is a good chance I'm missing other options out there too!

Any help much appreciated.

Cheers, Lid