Group: Forum Members
Posts: 550,
Visits: 27K
|
This highly depends on the shape of your specific seat. But something about 240g carbon twill, 200g carbon biaxial, 2-3mm soric (sf or better lrc), 200g carbon biaxial, 240g carbon twill might be what you are looking for. Light, but usually strong enough for tasks like that. Don't use sandwich materials at mounting points. Based on your question I might guess, that you haven't got much experience in structual composites. Remember that a seat is a safety critical part.
|