Hi Jan,
Unfortunately we do not have any tape or braid versions of the hybrid orange carbon fabric. You could cut the fabric into strips, but you would need to handle it carefully to avoid excessive fraying or use a hairspray to help bind the fabric so it does not fray so much when moved.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|