Orange-Black Kevlar-Carbon Tape/braid
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jan Christian
J
Jan Christian
posted 9 Years Ago
ANSWER
HOT
Topic Details
J
Group: Forum Members
Posts: 5,
Visits: 63
Hello! Is it possible to get something like this:
https://www.easycomposites.co.uk/232g-plain-weave-carbon-fibre-tape
or this
https://www.easycomposites.co.uk/aramid-flat-braid-tape-32mm
But in woven black-orange carbon-kevlar like this:
https://www.easycomposites.co.uk/carbon-fibre-cloth/hybrid-and-decorative-carbon-fabrics/22-twill-210gsm-3k-1m-ORANGE.html
Probably impossible but just got to ask
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Orange-Black Kevlar-Carbon Tape/braid
Jan Christian
-
9 Years Ago
Hi Jan, Unfortunately we do not have any tape or braid versions of the hybrid orange carbon fabric. You could cut the fabric into strips, but you would need to handle it carefully to avoid excessive...
Warren (Staff)
-
9 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search