Its hard to tell in the pictures. I presume the white lumps are the stones?
If so the remaining cloudiness could be either moisture reaction., or the resin having got very cold due to low temperature.
If it is moisture , getting the room dry and warm may help if the cure hasn't gone too far but usually it is too late once it has gone hard.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|