Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
It depends how precise. If fitting isn't too critical then wait until the end. Otherwise after the first layer of resin at the de-nib stage, you can cut them then and subsequently as you add layers of resin, it will thin around those hole edges both naturally and due to sanding.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|