Hi, I am using the gelcoat gun for the first time. I am trying it with a white low viscosity polyester gelcoat designed for spraying. The gelcoat manufacturer recommends 2-3mm spray nozzle at a 5-bar pressure, so I am using FN3 (2.4mm) nozzle. The cup is half full and you can see on the video that there are small drops falling from the nozzle when not spraying which I think is OK. However, when I pull the trigger, very little gelcoat is flowing, just the first drop. I tried to increase the pressure up to 8 bars and it's all the same - no gelcoat is flowing, just the air at a high pressure. The compressor is 256 l/min (9 cfm), 10 bar. Do you have any idea what's wrong?



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search