Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Not uncommon to find no post-cure data, but generally you should always be able to find a 'Tg' or 'HDT' value, which is the upper temperature limits of the resin. For most entry level epoxies this is around 60 degrees.
If you can't find any data at all, I would hazard a guess at it being around a 60 degree Tg, so you could do a post-cure of 60 degrees for 16 hours. Ideally you would ramp up to this temperature slowly, 0.5-1 degree per minute.
|