have a look at alan harper composites, they do silicone reusable bags.
We are hopefully getting one of there systems soon to play with.
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Hi guys does anyone have any links on making a reusable vac bag?  I'll only be using it for skinning parts to hold the cloth in place while the Base coat drys.
Also any better ways to seal the bags?  Using the easy composites bag putty tape just now but finding it hard to fully seal.
Would those plastic bag tools work that melt the 2 bags together? 

Cheers