I'm trying to infuse a new part, however I have doubts on the best location for my resin entry line.

At the moment I placed the vacuum line around the entire flange of the mold and the resin inlet in the center with spiraduto assisting in the distribution throughout the piece because it is of average size with 1.30 m in length.

Is this location in the vacuum and resin lines good, or is it interesting to change the location?

Before I left the resin inlet on one side of the length and the vacuum on the other side on the flange for the resin to travel the shortest distance, however had dry areas because the resin did not distribute perfectly.

Ps: I use resin w/ gel time of 30 minutes. 

This piece is a rear spoiler, see that the vacuum lines are skirting the flange and the resin inlet line is centered with spiraduto across the entire center length.


The resin inlet hose has not yet been loaded at the time of the photo.