Woven Glass dimension


Author
Message
GorVel
GorVel
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 2, Visits: 6
Thanks A lot
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi GorVel,

All our fabrics are sold by the linear metre which means that if you buy a quantity of "1" then you would receive a piece of material that is 1m wide (the stated width) and 1m long (the Qty 1). The weight of the fabric is 163g per square metre (g/sm).

I hope this explains it for you.

Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GorVel
GorVel
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 2, Visits: 6
Hi there,

Can anyone tell me what dimensions is one sheet (unit) of woven glass. 1 meter wide and 163g (long???) is bit of strange terminology for fabric...