Group: Forum Members
Posts: 74,
Visits: 1.8K
|
I'm setting up a production line for some small to medium size cosmetic parts and I'm having a question as to which manufacturing process to use.
Hand layup (w/ Vacuum Bag) or Vacuum Process Infusion ? Which of these processes will be faster to produce parts on average of 20 units / day with a low cost and good cosmetic quality?
I've been doing some things through the infusion process, but I see that the setup time of the mold and the whole infusion system ends up holding me too much in one piece.
|