Hi

I was attempting to make a mould for a car hatch/boot and ran into what i presume are a couple of problems in that i applied the gel coat, catalysed at 1.5%,, after reading the instructions that indicated you should leave till tacky or overnight i was surprised that in under two hours the gel was dry to the touch in places with no tack at all.  At this time i did what was probably the wrong thing and decided to put the coupling coat on, which again went past the tacky stage in places before i'd noticed so i put the reinforcing on.

my question is, can you 'rescue' the job if you get a cure before the next layer goes on, should the job be abandoned or is it not a major problem?  in truth i will probably only ever pull two or three products from the mould so long term durability isnt an issue.

Thank you for your time