Hi Guys! 

I have some problems with fixing two parts. They're aesthetic piece, this limits what to do and use to fix them.

Any suggestions for this application?

Example: 

http://www.talkcomposites.com/Uploads/Images/3c3c2a2a-6e75-41af-8ad0-0f68.png
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can bond along the seam but it would be inherently weak.  A solution is to bond the seam, then hand laminate some carbon fibre tape over the inside of the join to give you the strength.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
what warren said, or you could see about adding a joggle into the tool to allow a nice bonding area on the two parts.


Dezer
Dezer
Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)Supreme Being (698 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
I did tests using Plexus MA 310 (Methacrylate) with black pigment, the problem is after drying I could not remove the excess, especially in parts with geometries with more limited access internally.

When making the reinforcement with CF internally, this hinders me because it changes the internal dimension of the part.

I need to learn how to make pipes with complex geometries in another way without being in two parts.
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
If you are looking at making pipes in one piece then you need to be looking at mandrels or soluble tooling that you wrap the material around, braided socks are especially good at this process and a lot quicker than trying to apply single tows or pieces of material.

I used to make a lot of fuel and coolant carbon hoses for F1, the tools were 3d printed and then wrapped in prepreg then placed into a composite mould so both internal and external faces were tooled, expensive but it had the results we required.
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Out of interest,  what sort of wall thickness was needed for the engine coolant pipework?

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
they were about 2mm thick iirc