Sealing MDF moulds for vinylester resin infusions


Author
Message
SkiFreak
SkiFreak
Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)
Group: Forum Members
Posts: 9, Visits: 122
FLD (13/06/2017)
I've never used the bespoke products as I'm too tight but I've heard they're all pretty good.

I hear ya. I am in a very similar boat myself. Smile
What did you use as a mould sealer?


Hanaldo (13/06/2017)
Gelcoat would bond fine, but it wouldn't be the easiest thing to get a smooth surface with.

I agree, and it is a real pain to sand too, but as I have mentioned, I am looking at all possible options at this point.
If I can find something that works well, and does not cost a fortune, that is what I will be using.

I am in Australia, but I do know where I can source Duartec products and have thought about using this, if all else fails.