Nail varnish remover is just watered down acetone with perfumes added.  A good substitute if you want small quantities and can't find a local industrial supplier of acetone.  Most supermarkets or similar will have a budget nail varnish remover which is fine for the job.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Brilliant, thanks Warren!
NTF6
NTF6
Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)
Group: Forum Members
Posts: 13, Visits: 34
I would've thought that if it has been sanded down with 120 grit ready for the next coat then there shouldn't be anything clean off the surface, i just washed mine in clean water once it was keyed with 120 and then when it was dry applied then next coats.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In theory, once heavily keyed, there should be no original surface left, but it depends on nature of contaminant etc so by using a solvent as well to be sure you should be fine.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search