By Junior - 5/29/2017 6:34:40 PM

Do you have to use acetone to clean in between layers of laminate, or is there something else I can use to clean after sanding?
By Warren (Staff) - 6/2/2017 9:00:50 AM

In theory, once heavily keyed, there should be no original surface left, but it depends on nature of contaminant etc so by using a solvent as well to be sure you should be fine.