Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
I would also tighten up on your weighing and mixing as slight errors in these can all contribute to the problems you are having. When the mix ratio or mixing itself is out, the cured hardener components can come to the surface as with blushing causing the same problems.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|