Xcr resin goes white when wet sanded


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If the resin is going white when wet sanding then that is due to the resin not being fully cured before sanding.  Uncured epoxies are hydroscopic until cured so what tends to happen is the moisture makes the resin surface cloudy as it is absorbed. 

I would leave your parts longer to cure to be on the safe side. If that doesn't solve it, have a look at your mixing ratio and batch size to ensure you are within 1% accuracy to ensure things fully cure.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
It's just what there how too video shows you to you buddy,  but  yeah I think I might try that,  prefer wet sanding but it's clouding the resin :s
rmaddock
rmaddock
Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)Supreme Being (146 reputation)
Group: Forum Members
Posts: 17, Visits: 1.5K
I've no idea about the colour change, but why not use some finer sandpaper after the 120? 120 seems rather fierce for creating a key for the next coat.
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Anyone know why this happens?  My parts are cured and.when I wet sand the resin goes white,  reason I wet sand is the 120 grit tends to leave marks.that can be seen after another coat of resin.