Any advice on how to make a nice looking snorkel (straight tube) out of CF its 4.5" (114mm) outside diameter and 4" / 100mm long.

I tried wet lay-up round a sacrifical former with vac bag film over the top taping round it to provide some tension.
The layers consolidated fine, result is ok but not super smooth (although I haven't gelcoated it yet).

I could make a mould at 117mm id but I expect it would be hard to neatly place 3 layers of CF and then a pain to vac bag.
I could retry the former route and seal it to pull a vacuum (former would need to be fairly strong I guess which would add to the release challenge).

Is it feasible to get a good finish with wet layup and vac bag film pulled tight round the part?
Its not really on show so maybe I'm being over fussy.

Any views appreciated!

Thanks
Stuart
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search