Hi guys I'm thinking of making my car dashboard in CF, I started with a small piece on the left side of the steering wheel. The piece is good enough but I do not know how to fix into the car .. i do not know the correct name of it (clips, tooth, plastic caps) but how can i create it ?? Or, if you have other ways please explain Me Smile
Here 2 photos of the piece, the car is an Abarth grande punto , and no, I'm not going to skin it !!
Attachments
IMG_1088-min.jpeg (1.1K views, 905.00 KB)
IMG_1089-min.jpeg (982 views, 659.00 KB)
Edited 9 Years Ago by SUPERTIA
Carbonphoenix
Carbonphoenix
Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)Supreme Being (155 reputation)
Group: Forum Members
Posts: 12, Visits: 134
SUPERTIA - 4/21/2017 11:41:03 AM
Hi guys I'm thinking of making my car dashboard in CF, I started with a small piece on the left side of the steering wheel. The piece is good enough but I do not know how to fix into the car .. i do not know the correct name of it (clips, tooth, plastic caps) but how can i create it ?? Or, if you have other ways please explain Me Smile
Here 2 photos of the piece, the car is an Abarth grande punto , and no, I'm not going to skin it !!

I know what you mean, I also trying to find the answer to this.
I think it needs another cast but of the underside and the two layers bonded together?

Saff
Saff
Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)Supreme Being (138 reputation)
Group: Forum Members
Posts: 10, Visits: 723
For a similar piece I glued some piece of plastic tube on the backside of the part. The inner diameter was similar to the diameter of the clip, so it worked fime!


my facebook page
Pravin Kumar
Pravin Kumar
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 1, Visits: 2
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search