I'm a little confused with something and wondered if someone could enlighten me...

The recommended ratio of resin to fabric for fibreglass and Carbon Fibre appears to be the same i.e. 200g of resin for 200g of fabric, so when people say the same product made in carbon would weigh less as it requires less resin, how can this be?Blink