	Group: Forum Members 	        
    Posts: 135, 
    Visits: 1.6K 
    
 
          
		     | 
				                       
                 
                
                    
			            As Matt was saying, for polypropylene sheet and PTFE you dont need any release agent, as the epoxy will not stick to it at all. 
  Are you planning to make flat sheets of material? Then your definitely best with a sheet of glass, coated with easy-lease as a mould. It can be re-used indefinitely, unlike the other materials which will become scratched quite quickly which will be visible in your surface finish. 