Casting with glow in the dark (Tutorial)


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A good video as always Matthieu!  It is quite good you managed to get the particles fairly even in the resin. I have seen some glow in the dark castings were it all went wrong!!

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi everyone! 
Just uploaded a new tutorial on my youtube channel that might be of some interest for some of you
1. Casting VAC CAST epoxy resin
2. silicone casting
3. casting clear pieces with IN2 Infusion resin(!)
4. using 3D-core to make sandwich panel
5. bonding pieces

Have fun and discuss on in the comment section below the video 
or down here Wink

 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com