I want to place a part made with PX6 into a mould and use PX90 around the part to set around it. I have designed the part with features to hold onto the PX90. Will the PX90 adhere to the PX6 part if I rough the surface up or do I need to place some adhesive around the part to adhere it to the PX90 ?
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Generally PU bonds to PU in cases like this, however it is not one I have tested personally.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search