I am rebuilding a Ducati Monster M900 1994 into a café racer. My object is to reduce the weight of the bike by about 25kg and increase the power by about 10%.
I have started with the seat and made the male mould.  This is awaiting final finishing and polishing before I make the female mould in 2 parts. I will use wet lay up as I do not have the vacuum equipment. The garage is too cold to do any resin work at the moment and it also needs a good vacuuming to remove all the filler material sanded off from the tank mould, still another 6 cycles of filling and rubbing down before this is ready for mould primer resin   

              IMG_0789 seat former 2.JPG              (0 views,              581.11 KB)                            
              IMG_0788 seat former.JPG              (0 views,              480.90 KB)                            
              IMG_0867.JPG              (0 views,              521.68 KB)                            
              IMG_0904.JPG              (0 views,              490.04 KB)                            
              Tank plug 2.jpg              (0 views,              626.63 KB)                            
              seat plug.jpg              (0 views,              448.64 KB)                            
              Tank base plug.jpg              (0 views,              544.95 KB)                            
              Tank airbox glued.JPG              (0 views,              460.69 KB)                            
              IMG_1196.JPG              (0 views,              579.72 KB)






Edited 9 Years Ago by Warren (Staff)
Dravis
Dravis
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Something gets screwed up in this thread ... You can not click on the images, when you try a new EC home page opensCrazy
 

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I have had a play with your post and got rid of some of the corruption and spacing but cannot recover the image links. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search