PVA release agent - how long before applying epoxy gelcoat?
PVA release agent - how long before applying epoxy gelcoat?
Post Reply
Like
3
PVA release agent - how long before applying epoxy gelcoat?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Christian_83
Christian_83
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 70
Hi Guys
Im trying to make a mold of an existing part /that i use as a plug)
Ive given the part 5 times of carnauba wax and then 2 coats of PVA (20 min cure between layer) I didn't have the time to put on the epoxy tooling gelcoat.
So my question is, will the PVA still "work" if i put on the epoxy tooling gel coat in 24 hours? or will i need to put on new PVA?
Is there any reason with applying more than one layer of PVA (to be sure that all corners and fed ) ?
Cheers
Christian
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
No time limit as such, you just want to apply it before it gets covered in dust or other possible contamination, and beware of the PVA shrinking in places and cracking or pulling away from the surface.
Other than that, you could apply the gelcoat 6 months later and it wouldn't be a problem.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search