Mig
Mig
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 16
Hello,
I have got a very small cracks on my multicopter landing gear made of carbon fibre K3. The cracks are by the middle guided holes on the port side of the landing gear and although there are very small cracks I would like to know if they could be reinforced or fix with one of your products.
Could you please recommend which one will work better in this kind of cracks.
Regards
Miguel
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Multicopter landing gear
Mig
-
14 Years Ago
Hi Miguel, Yes, I would certainly say it would not be difficult to do some local reinforcement of...
Matt (Staff)
-
14 Years Ago
Thanks a lot Matt for your advice. I will do as you recommend. With regards Miguel
Mig
-
14 Years Ago
Just one stupid question, when you are saying to use EL- 2 Laminating Epoxy to wet the fibre, are...
Mig
-
14 Years Ago
Hi Miguel, Yes, certainly. Whenever we talk about using epoxy resins for laminating, coating,...
Matt (Staff)
-
14 Years Ago
OK thanks a lot for your time and info. Mig
Mig
-
14 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search