Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Degassing
Degassing
Post Reply
Like
3
Degassing
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Umang
Umang
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 7
Why is degassing needed??
Is it needed if we do vacuum bagging with hand layup.
What happens when we degas ??
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Degassing
Umang
-
10 Years Ago
Hi, Degassing just removes the air trapped in the resin mixture as quite a lot of air gets trapped...
davro
-
10 Years Ago
There's no real point in degassing before wet-laying, it's virtually impossible to not introduce air...
Hanaldo
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search