Message
joellawtie
joellawtie
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 20,
Visits: 223
Hey Kirk ,
I would agree with what Davro says.
I tried skinning and even small parts can take 2 weeks to perfect. Like i did my ignition barrel and even that has a fitting issue so doing panel edges would cause a lot of issues and if you want it as a demo car would you really want scuffed carbon etc?
If you are starting carbon parts / skinning as a company service you better have a lot of time and patience and the best of conditions for letting the epoxy cure.
any moisture in your garage will ruin the coat i have first hand experience with this and it's devastating.
You say about wanting to do skinning instead of infusion and prepreg because of cost but skinning parts will never be as good quality and infusion/prepreg and if i was running a business quality is everything.
If you did get into making molds you can get into pattern making and then your demo car could have custom made body parts exclusive to that car and your company.
I will be doing a full carbon makeover of my car when i have the time away from work and ill be doing it with infusion.
Reply
Like
6
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
Hi fasta will u be a your unit tomorrow
And I'll pop in ?
Cheers graham
Reply
Like
6
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I'll be there first thing in the morning hour or so from 9am.
40 deg C public holiday, too hot for work.
Fastacraft Facebook page
Edited
9 Years Ago by
Fasta
Reply
Like
6
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
Cool see u at 9 am I forget it's a holiday
Reply
Like
5
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
That duratec tec sun sheid is great look at the finish
Thanks fasta for giving me some to try
How long dose it take to dry It still seams
Tacky but hard if u no what I mean
Attachments
IMG_4659.JPG
(
290 views,
541.00 KB
)
Reply
Like
7
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Assuming the catalyst was the right one then it should be ok overnight to sand.
Fastacraft Facebook page
Reply
Like
6
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
Just the mekp one I used from kirkside
Is that the right one Fasta.
Reply
Like
7
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
The MEKP from Kirkside will work fine mate.
Reply
Like
5
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
Yes it dryed and jeso it's easy to flatten back. great product
Has any one tryed kbs Dimond clear coat
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Prev
1
2
3
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search