The Uni-Mould system is very good for out of autoclave pre-preg work as long as you keep to the limits of the system. We have Uni-Mould moulds for various pieces that literally have had over a hundred pulls off them with only an occasional polish needed to maintain surface gloss.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|