Group: Forum Members
Posts: 3,
Visits: 55
|
Hi, again
Idea about Hammerite was very bad, because after two days I tried to clean it with acetone and its simply washed off. So I sanded surface with 60 grit paper and paint it over with polyester resin. Sand it up to 1200 grit, but when i put on masking tape to make flanges, polyester cout came off with tape.
Its old Honda CF70 mudguard, so lot of dents and scratches, thats mean I need for filler to get nice shape. Can somebody recomend whitch filler to use and what to paint over it to get nice surface?
And can I use fiberglass laminate sheets for flanges instread of sign board or something like that.
Thanks Andris
p.s sorry about my bad english.
|