Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Easy-Lease & Masking Tape
Easy-Lease & Masking Tape
Post Reply
Like
3
Easy-Lease & Masking Tape
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Imiq Paddle Sports
Imiq Paddle Sports
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 63
I would like to mask out a design on a mold prior to spraying gelcoat.
Are there any known issues with the adhesive from masking tape that would impair the properties of Easy-Lease?
Also, is there a more appropriate tape to use i.e; automotive masking tape for pin striping etc.
All advices greatly appreciated.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Easy-Lease & Masking Tape
Imiq Paddle Sports
-
9 Years Ago
It won't affect the release properties at all, but you will want to be aware the masking tape will...
Hanaldo
-
9 Years Ago
I have had very poor luck with using any of my masking-tapes on an "Easy-Leased" surface -- But: You...
Dravis
-
9 Years Ago
Yeh it's not easy at all. It can be done though, it's something I do fairly regularly. Took me 4 or...
Hanaldo
-
9 Years Ago
Thanks Composite Masters!! I'll share some pre & post photos. Imiq
Imiq Paddle Sports
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search