Group: Forum Members
Posts: 592,
Visits: 1.9K
|
IMHO a 2 mm thick (Even a 1,5 mm ) solid carbon/kevlar mixed panel/flor plate will outperform the original 1 mm aluminum, it will certainly be just as stiff, provided that you lay up with some of the CF/kevlar at 45 deg . (or buy some of the cheap biaxial that EC has on sale .. great stuff .. )
a 2 mm Infused CF panel will use about 8 layers of 200 gsm CF cloth -- I would go for 2 -3 layers of "outside" in the pattern you want and then 2 layers of 300 gsm biaxial -- That will certainly be just as strong as a 1 mm alu plate ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|